# Perforated tear-off layer for 3D printing: one-time pull-tab lids, sealed capsules, breakaway supports (STL, STEP)

> How do I 3D print a lid or support that tears off cleanly in one piece, like a one-time pull tab?

- Category: 3D printing › Techniques
- Kind: Hardware
- Basis: Xem technique. A layer of dots that the next layer bridges, used as a designed weak plane; related to tamper-evident designs that use stress concentrators and pause-and-insert containers (MakerWorld), and to support interface / contact-distance settings (Prusa, OrcaSlicer).
- Page: https://xemstudio.com/objects/perforated-tear-off-layer/ · JSON: https://xemstudio.com/api/geometry?object=perforated-tear-off-layer · Plain text: https://xemstudio.com/objects/perforated-tear-off-layer/sheet.txt
- License: dimension sheet CC BY 4.0 (Xem Studio); files Xem Studio Design License (free to use and sell from, not to redistribute as files: https://xemstudio.com/license/)
- Use in every chat: add https://xemstudio.com/mcp as a connector (https://xemstudio.com/use-with-ai/)

## Overall (mm)

| length | width | height |
|---|---|---|
| 72 | 60 | 41.8 |

**Exact dimensions.** Every file is drawn at true size with no tolerance added. The holes and pins that meet another part are listed below under Mating features, with the fit each joint needs; open those by your process's clearance before making the part.

## Notes

- Starting values, not tested limits: 0.2 mm layer height, dots Ø0.8 mm at 2 mm pitch, exactly one layer tall, on a layer boundary (z a multiple of 0.2). Print the test strip first and pick the pitch that holds but tears cleanly.
- Smaller pitch or bigger dots = stronger seal; wider pitch tears more easily.
- Load a container: pause the print at the dotted layer's height, drop the item in, resume. The lid bridges the opening, so keep it under about 40 mm across or tune bridge settings.
- Breakaway support: keep the 0.4 mm side gap to the part and turn slicer supports off for that region.
- Tiny dots depend on the slicer: check the preview shows them; if it drops them, use 1.0 mm dots or turn off small-gap filtering.

## Mating features (exact size; open press / slide / run / socket by your process clearance, leave designed and clamp as drawn)

| feature | exact | mates with | fit | files |
|---|---|---|---|---|
| dotted seal layer | Ø0.8 dots, 2 mm pitch, 1 layer | lid / tab / support above it | designed | all |

## Sizes

| file | what | overall mm |
|---|---|---|
| perf-tab-box-40 | 40 × 40 × 20 mm one-time box: lid held by 76 dots (Ø0.8, 2 mm pitch, one 0.2 mm layer) on the wall tops, upright pull tab. Pause at z = 20 mm to load it | 40 × 40 × 31.8 |
| perf-tab-box-60x40 | 60 × 40 × 30 mm one-time box, same dotted seal; pause at z = 30 mm | 60 × 40 × 41.8 |
| perf-capsule-30 | Ø30 × 25 mm round capsule, dotted rim seal, pull-tab lid; pause at z = 25 mm | 30 × 30 × 36.8 |
| perf-breakaway-support-coupon | Breakaway support test: 30 mm overhang on a support block joined only by one dotted layer, 0.4 mm off the post | 40 × 20 × 23 |
| perf-test-strip | Calibration strip: three pull tabs on dotted layers at 1.5, 2 and 3 mm pitch | 72 × 22 × 12.2 |

## Where the files are

- MakerWorld: [Tamper Evident Seal with Container](https://makerworld.com/models/1288041) — web — Publisher's page; dimensions are facts
- Prusa Research: [Support material (contact Z distance, interface layers)](https://help.prusa3d.com/article/support-material_1698) — web — Publisher's page; dimensions are facts
- OrcaSlicer: [Support Advanced: Z distance, interface spacing](https://www.orcaslicer.com/wiki/print_settings/support/support_settings_advanced.html) — web — Publisher's page; dimensions are facts

## Free STEP/STL (5 parts, Xem Studio Design License, Xem Studio)

Index: https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/index.json · license: https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/LICENSE.md

- perf-tab-box-40: [STEP](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-tab-box-40.step) · [STL](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-tab-box-40.stl) — 40 × 40 × 20 mm one-time box: lid held by 76 dots (Ø0.8, 2 mm pitch, one 0.2 mm layer) on the wall tops, upright pull tab. Pause at z = 20 mm to load it
- perf-tab-box-60x40: [STEP](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-tab-box-60x40.step) · [STL](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-tab-box-60x40.stl) — 60 × 40 × 30 mm one-time box, same dotted seal; pause at z = 30 mm
- perf-capsule-30: [STEP](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-capsule-30.step) · [STL](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-capsule-30.stl) — Ø30 × 25 mm round capsule, dotted rim seal, pull-tab lid; pause at z = 25 mm
- perf-breakaway-support-coupon: [STEP](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-breakaway-support-coupon.step) · [STL](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-breakaway-support-coupon.stl) — Breakaway support test: 30 mm overhang on a support block joined only by one dotted layer, 0.4 mm off the post
- perf-test-strip: [STEP](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-test-strip.step) · [STL](https://xemstudio.com/files/3d-printing/perforated-tear-off-layer/perf-test-strip.stl) — Calibration strip: three pull tabs on dotted layers at 1.5, 2 and 3 mm pitch

## Questions

**How do I make a 3D printed tear-off tab?**

Join the tab with one layer of dots instead of a solid layer. The next layer bridges the dots; pulling the tab breaks them along that layer.

**How do I print something inside a sealed container?**

Pause the print at the dotted layer height, drop the item in, and resume. The lid prints over it and only opens by tearing the seal.

**Can this replace normal supports?**

For a block under a flat overhang, yes: a support block joined by one dotted layer snaps off in one piece with little cleanup.

**What dot size and spacing should I use?**

Start at Ø0.8 mm dots, 2 mm apart, one 0.2 mm layer, then tune with the test strip for your filament.

**Is it tamper evident?**

Yes: once torn the dots can't be rejoined, so an opened lid is obvious.

## Fits with

- [3D printable snap-fit hooks and catches: cantilever latch, permanent or releasable, 4 sizes (STL, STEP)](https://xemstudio.com/objects/snap-fit-hooks-and-catches/)
- [3D printable annular snap-fit caps and containers: push-on lid with bead and groove, 20–50 mm (STL, STEP)](https://xemstudio.com/objects/annular-snap-fit-caps/)
- [Living hinge (flexure hinge)](https://xemstudio.com/objects/living-hinge/)
- [Print-in-place: push button with flexure return and click](https://xemstudio.com/objects/print-in-place-push-button-flexure/)